MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior Wrap Core Flux Rosin Fully Activated Core Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • RA Flux for loading into core solder.
  • Conforms to ANSI-J-STD-004, Type ROL1.
  • Excellent for general purpose electronic and non-electronic soldering applications.
Description: Superior WRAP Core Solder Flux is a Rosin Fully Activated (RA) type of core flux specifically formulated for manufacturing RA type core wire solders of 1.1 – 3.3% flux loading. Superior WRAP Core Solder Flux is formulated to meet the requirements of J-STD and IPC specifications. This flux is designed to meet the requirements of many electronic soldering assembly applications and provides increased activity to improve solderability. Flux residues can be removed by solvent cleaning or by saponification cleaning.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
ColorAmber
FormSolid
Water Extract Resistivity>60000 ohm/cm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSFLUX137 / 185821

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.