MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lehvoss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK with carbon fiber, PTFE, lubricant modified  (discontinued **)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Properties/attributes include: Strong, stiff parts; low thermal coefficient of expansion. Dynamically-stressed parts moving at high velocity. Chemically- and hydrolytically- resistant parts, non flammable. Improved friction and wear behavior, self-lubricating, for highest tribological requirements.

Automotive industry, textile machinery, medical- and precision engineering, aircraft industry. Typical uses include: Bearings, sleeves, control disks, gear wheels, pump impellers, gear parts.

Processing: During processing, the moisture content should not exceed 0.05%. To avoid internal stresses, a medium to high injection rate should be used. An increase in tool temperature may be helpful. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmDIN 16901
Melt Flow <= 10 g/10 min
@Load 10.0 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 155 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Modulus of Elasticity 13.0 GPaISO 527-2
Flexural Strength 210 MPaISO 178
Flexural Modulus 9.00 GPaISO 178
Flexural Strain at Break 3.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 25.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 30.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1fu
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179 eA
 7.00 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1.00e+8 ohm-cmIEC 60167
Surface Resistance <= 1.00e+7 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CDIN 53752
Thermal Conductivity 0.450 W/m-KDIN 52612
Maximum Service Temperature, Air 250 °CContinuous; UL 746B
 280 °CShort Term
Deflection Temperature at 1.8 MPa (264 psi) 260 °CISO 75-2/A
Vicat Softening Point 300 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 360 - 380 °C
Zone 1 360 - 370 °C
Zone 2 380 - 390 °C
Zone 3 390 - 400 °C
Melt Temperature 390 °C
Mold Temperature 170 - 190 °CSuggested Range
Drying Temperature 120 °C
@Time 21600 - 28800 sec
Dehumidifying dryer
 150 °C
@Time 10800 - 21600 sec
Dehumidifying dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
Colornatural color (black)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehvoss LUVOCOM® 1105/GR/15/TF/15-2 PEEK with PTFE, lubricant modified
Evonik Vestoran® 1300-GF20 nf PPE
Evonik Vestoran® 1300-GF10 nf PPE
Lehvoss LUVOCOM® 1105/GF/20/EM PEEK with glass fiber
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE

PLUU8819 / 193778

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.