MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Matexcel CER-0065 Ceramic fiber blankets
Categories: Ceramic

Material Notes: Ceramic fiber blanket has high tensile strength and low shrinkage. It has great resiliency with low heat storage. This product has low thermal conductivity and great resistance to thermal shock as well as great sound absorption.

Ceramic fiber blankets

Application: – Furnace repair – Furnace, kiln, reformer and boiler linings – Furnace door linings and seals – Reusable insulation for steam and gas turbines – High temperature insulation for kiln and furnace – Primary reformer heater insulation – High temperature insulation gaskets – Expansion joint seals – Glass furnace crown insulation – Field steam generator lining – Nuclear insulation applications – Thermal reactor insulation – Flexible high temperature pipe insulation – Investment casting mold wrapping – Removable casting mold wrapping – Removable insulating blankets for stress relieving welds – Pressure and cryogenic vessel fire protection – Soaking pit seals – High temperature filtration

Key Words: Synonyms: Ceramic fiber blankets
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 12700 - 50800 microns500 - 2000 mil
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1260 °C2300 °F
 1360 °C2480 °F
 1400 °C2550 °F
 1430 °C2610 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1502 / 300133

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.