MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa JH820 Modified PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes:
    Features:
  • Excellent balance properties
  • Super high impact strength
  • High stiffness
  • Good size stability
  • Good surface, high gloss
  • High transparency

    Applications:
  • Injection molding
  • Household appliance
  • Business machine cabinet
  • Transparent plate
  • Packaging

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/cc
@Temperature 23.0 °C
ASTM D792
Water Absorption 0.12 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 62.0 MPa50mm/min; ASTM D638
Elongation at Break 100 %50mm/min; ASTM D638
Flexural Strength 85.0 MPa2mm/min; ASTM D790
Flexural Modulus 2300 MPa2mm/min; ASTM D790
Izod Impact, Notched 700 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmASTM D257
Dielectric Strength 28.0 kV/mm1.6mm; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 3.20 mm
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
Rear Barrel Temperature 240 - 270 °CStart Point: 260°C
Middle Barrel Temperature 260 - 280 °CStart Point: 265°C
Front Barrel Temperature 270 - 290 °CStart Point: 275°C
Melt Temperature 250 - 280 °CStart Point: 260°C
Mold Temperature 60.0 - 80.0 °CStart Point: 70°C
Drying Temperature 120 °C
@Time 14400 - 21600 sec
Pre-dry
Back Pressure 0.700 - 1.00 MPa
 
Descriptive Properties
Injection Speed60-90%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa JH830 Flame Retardant PC
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance
Covestro Apec® RW1697 Polycarbonate
Kingfa JH830T Flame Retardant PC

PKINGF049 / 104308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.