HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPE Application: Agrochemical Container, SORE* Fuel Tank, PFC CAS No. 9002-88-4 and 25038- 54- 4 Information provided by LG Chemical |