MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV 2455-1 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TVP 2455-1 is a high performance thermoplastic vulcanizate used in variety of consumer and industrial applications, including seals and gaskets, where copper stabilization is required. Sarlink TVP 2455-1 is a medium hardness, low density grade with good resiliency and compression set designed for injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Copper Contact Stabilized; Good Adhesion; Good Processability; Low Density; Medium Hardness; Low Specific Gravity; Resilient

Uses: Gaskets; Glazing; Grommets; House; Industrial Applications; Plugs; Rubber Replacement; Seals

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55ASTM D2240
Tensile Strength at Break 540 psiASTM D412
Tensile Stress at Strain 300 psi
@Strain 100 %
ASTM D412
Elongation at Break 300 %ASTM D412
Tear Strength 110 pliASTM D624
Compression Set 22 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395B
 42 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 374 - 446 °FInjection, Melt
Rear Barrel Temperature 344 - 416 °FInjection
Middle Barrel Temperature 354 - 426 °FInjection
Front Barrel Temperature 364 - 436 °FInjection
Nozzle Temperature 374 - 446 °FInjection
Zone 1 330 - 400 °FExtrusion
Zone 2 340 - 410 °FExtrusion
Zone 3 350 - 420 °FExtrusion
Zone 4 351 - 421 °FExtrusion
Zone 5 360 - 430 °FExtrusion
Die Temperature 374 - 440 °FExtrusion
Mold Temperature 95.0 - 140 °FInjection
Drying Temperature 176 °F
Dry Time 3.00 hour
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 125 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Vyram™ 9101-45 Thermoplastic Elastomer
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer
Teknor Apex Telcar® OBC 2419A Thermoplastic Elastomer
Mitsui Milastomer™ M3800BS Black Vulcanized Thermoplastic Elastomer
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer

PTEKNQ1130 / 237621

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.