MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Encom Polymers EnLon F0PX30GF Amorphous Nylon, 30% Glass Filled, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Amorphous Nylon

Material Notes: Appearance: Black Color Only

Processing Methods: Injection Molding

Applications: Highly Engineered FR Polymer suitable for Die Cast Replacement

Information provided by EnCom Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccASTM D792
Filler Content 30 %30 %
Water Absorption 0.20 %0.20 %ASTM D570
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage, Flow 0.0060 cm/cm
@Thickness 3.20 mm
0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 41 g/10 min
@Load 2.16 kg,
Temperature 275 °C
41 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 12.069 GPa1750.5 ksiASTM D638
Flexural Strength 286 MPa41500 psiASTM D790
Flexural Modulus 11.586 GPa1680.4 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 237 °C459 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 224 °C435 °FASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 °C518 °F
Middle Barrel Temperature 275 °C527 °F
Front Barrel Temperature 280 °C536 °F
Nozzle Temperature 280 °C536 °F
Mold Temperature 120 - 140 °C248 - 284 °F
Drying Temperature 120 °C248 °F
Dry Time 2.00 - 12.0 hour2.00 - 12.0 hour
Screw Speed 60 - 150 rpm60 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENCOM016 / 266030

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.