MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
California Fine Wire Alloy 20-245 Precious Metal Alloy
Categories: Metal; Nonferrous Metal

Material Notes: All values may vary dependent on specific design and usage

Proprietary composition

Capabilities:

  • Wire
  • Insulated

Information provided by California Fine Wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.414 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 111000 psiStress relieved
 125000 psiHard
Modulus of Elasticity 9250 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 245 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Descriptive Properties
MagneticNone
Temperature Coefficient of ResistanceMax 0.00002 ohms/ohm-°C0-100°C
Thermal EMF vs. Copper-0.041 mV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reade Advanced Materials Wood's Metal Alloy (Sn + Pb + Bi + Cd)
316 Stainless Steel, annealed bar
304 Stainless Steel
ATI Allvac® Nickelvac® HC-276 Nickel Superalloy, Heat Treatment: 1121°C (2050°F) Anneal
Carlson 20 Plus Alloy

NCALZ10 / 15553

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.