MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Misumi Alumina 96 Aluminum Oxide, Al2O3
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by MISUMI Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.70 g/cc
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 300 MPa
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 9.0
Dielectric Strength >= 10.0 kV/mm
Dielectric Loss Index 0.00010
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.30 µm/m-°C
@Temperature 20.0 - 500 °C
 8.00 µm/m-°C
@Temperature 20.0 - 800 °C
Thermal Conductivity 18.0 W/m-K
Melting Point 2050 °C
Maximum Service Temperature, Air 1300 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 96 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Stainless Steel
Boron Nitride, Cubic BN, (Borazone)
Misumi Alumina 99 Aluminum Oxide, Al2O3
CeramTec 614/698 Alumina, 96%
Aremco Pyro-Putty™ 1000 High Temperature Ceramic-Metallic Putty, Aluminum Filled

CMISUM990 / 178111

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.