MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Miracll L95 Thermoplastic Polyurethane, Polycaprolactone Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Excellent hydrolytic resistance, oil resistance, good abrasion resistance, resilience, resilience performance, low temperature flexibility. Applications: oil seal, footwear, belting, hose & tube, wire & cable, wheel & caster, etc.

Information provided by Miracll Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9595ASTM D2240
Tensile Strength 50.0 MPa7250 psiASTM D412
Elongation at Break 400 %400 %ASTM D412
100% Modulus 17.0 MPa
@Strain 100 %
2470 psi
@Strain 100 %
ASTM D412
300% Modulus 32.0 MPa
@Strain 300 %
4640 psi
@Strain 300 %
ASTM D412
Tear Strength 170 kN/m970 pliASTM D624
Abrasion 3030DIN Abrasion Loss; DIN 53516
Compression Set  30 %
@Temperature 70.0 °C,
Time 79200 sec
30 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 42 %
@Temperature 100 °C,
Time 86400 sec
42 %
@Temperature 212 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -37.0 °C-34.6 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMIRAC55 / 221384

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.