Sandvik grade C9M has been specially developed for applications requiring high performance in corrosive environments. It combines corrosion resistance with high mechanical properties that can be utilized in a broad spectrum of the metal forming applications. Features: 9% alloyed nickel binder, 91% tungsten carbide. The grain size is fine.High resistance to corrosion due to the composition of the binder phase.Medium wear resistance.Good toughness.Information provided by Sandvik |