MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® Rx2635 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: MVR (300 °C/1.2 kg) 12 cm³/10 min; medical devices; suitable for sterilization with high-energy radiation; biocompatible according to many ISO 10993-1 test requirements; medium viscosity; easy release; injection molding - melt temperature 280 - 320 °C; available in color code 451118 only; transparent parts for medical devices

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.660 g/cc0.0238 lb/in³pellets; ISO 60
Density 1.20 g/cc0.0434 lb/in³ISO 1183-1
Moisture Absorption at Equilibrium 0.12 %0.12 %ISO 62, 50% RH
Water Absorption at Saturation 0.30 %0.30 %ISO 62
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inparallel/normal; b.o. ISO 2577
Melt Flow 13 g/10 min
@Load 1.20 kg,
Temperature 300 °C
13 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 5300 N
@Temperature 23.0 °C
1190 lb (f)
@Temperature 73.4 °F
ISO 6603-2
Tensile Strength at Break 75.0 MPa10900 psi50 mm/min; ISO 527-1,-2
Tensile Strength, Yield 67.0 MPa9720 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %Nominal, 50 mm/min; ISO 527-1,-2
 130 %130 %50 mm/min; b.o. ISO 527-1,-2
Elongation at Yield 6.1 %6.1 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527-1,-2
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Thickness 3.00 mm,
Temperature -30.0 °C
5.71 ft-lb/in²
@Thickness 0.118 in,
Temperature -22.0 °F
complete break; ISO 7391/b.o. ISO 180-A
 65.0 kJ/m²
@Thickness 3.00 mm,
Temperature 23.0 °C
30.9 ft-lb/in²
@Thickness 0.118 in,
Temperature 73.4 °F
partial break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
 NB
@Temperature -60.0 °C
NB
@Temperature -76.0 °F
ISO 179-1eU
Puncture Energy 60.0 J
@Temperature 23.0 °C
44.3 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 133 °C271 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FISO 75-1,-2
Vicat Softening Point 143 °C
@Load 5.10 kg
289 °F
@Load 11.2 lb
50°C/h; ISO 306
Flash Point 480 °C896 °FASTM D 1929
 550 °C1020 °Fself ignition; ASTM D 1929
 
Processing PropertiesMetricEnglishComments
Melt Temperature 290 °C554 °FInjection molding; ISO 294
Mold Temperature 80.0 °C176 °FInjection molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® XT5010 Polycarbonate
Covestro Bayblend® FR3012 PC/ABS Blend
Covestro Apec® HT KU 1-9343 High-Heat Polycarbonate, UV-Stabilized
Covestro Apec® HT KU 1-9331 High-Heat Polycarbonate
Covestro Apec® FR1892 High-Heat Polycarbonate

PB09650 / 150782

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.