MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 280 H Nylon 6, Heat Stabilized, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Impact Grade

Material Notes: Availability: Asia Pacific; Europe; North America

Additive: Heat Stabilizer; Impact Modifier

Features: Good Flexibility; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Impact Modified

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccASTM D792
Water Absorption 1.5 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.016 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8200 psiASTM D638
Elongation at Break 150 %ASTM D638
Flexural Strength 8500 psiASTM D790
Flexural Modulus 225000 psiASTM D790
Izod Impact, Notched 18.0 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 149 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 470 °F
Middle Barrel Temperature 450 °F
Front Barrel Temperature 440 °F
Nozzle Temperature 450 °F
Melt Temperature 428 °F
Mold Temperature 70.0 - 200 °F
Drying Temperature 150 - 180 °F
Injection Pressure 5000 - 20000 psi
Screw Speed 60 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecomid® NB40 NL IL PA6, impact modified, natural
Nurel Engineering Polymers Promyde® B30 P2 HI PA 6, Dry, Impact modified and Heat stabilized
Kingfa CPA-6 Toughened PA6
Envalior Akulon® K223-TP4 PA6-I, Dry, Impact Modified
Envalior Akulon® K223-TP4 (Dry) Impact Modified Nylon 6 (North America)

PTEKNQ0516 / 237007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.