MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 85XFS PA66/6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Vydyne 85XFS is a general purpose PA66/6 copolymer resin designed for extrusion-compounding applications. It is available in natural only. This copolymer resin provides a lower melting point and can be used for compounding thermally sensitive additives or fillers. It offers a well balanced combination of engineering properties characterized by high strength, rigidity, good toughness, high melt point, good surface lubricity, and abrasion resistance. Vydyne 85XFS exhibits chemical resistance to many chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Moisture Absorption 0.500 %ASTM D 6869
Viscosity Measurement 44 - 50Relative Viscosity; Formic Acid; ASTM D 789
 135 - 146Relative Viscosity; Sulfuric Acid; ISO 307
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 °CDAM; ISO 11357-3
 
Descriptive Properties
Agency RatingsEC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
AppearanceNatural Color
FeaturesAbrasion Resistance
 Chemical Resistant
 Copolymer
 Gasoline Resistant
 General Purpose
 Good Toughness
 High Rigidity
 High Strength
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific
Yellowness Index (YI)4ASTM D 1925

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9246 / 287599

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.