MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hapco DI- PAK™ E-4889 TPU
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: High performance, flexible potting systems designed to be in constant water immersion while maintaining electrical and physical properties. DI-PAK™ E-4888 & E-4889 were designed to meet Naval underwater applications.

The Di-Pak™ Advantage:

  • Flexible or Rigid
  • Low Viscosity
  • Multiple Speeds
  • Mercury Free
Improve your process and your product:
  • Eliminate Rejects
  • Fast Cure & Fast Turnover
  • Increase Performance
  • Hand Mix or Dispense

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccASTM D-4669
Viscosity 6000 cP6000 cPASTM D-4878
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787ASTM D-2240
Tensile Strength 13.1 MPa1900 psiASTM D-638
Elongation at Break 300 %300 %ASTM D-638
Modulus of Elasticity 0.0214 GPa3.10 ksiASTM D-638
Izod Impact, Notched NBNBASTM D-256
Izod Impact, Unnotched NBNBASTM D-256
Tear Strength 66.6 kN/m380 pliASTM 624 Die-C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.30e+16 ohm-cm1.30e+16 ohm-cmASTM D-270
Dielectric Constant  2.5
@Frequency 100000 Hz
2.5
@Frequency 100000 Hz
ASTM D-150
 2.7
@Frequency 1000 Hz
2.7
@Frequency 1000 Hz
ASTM D-150
Dielectric Strength 25.4 kV/mm645 kV/inASTM D-149
Dissipation Factor 0.036
@Frequency 100000 Hz
0.036
@Frequency 100000 Hz
ASTM D-150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.245 W/m-K1.70 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 110 °C230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min
@Thickness 3.17 mm
8.00 - 12.0 hour
@Thickness 0.125 in
Demold
Gel Time 25.0 min
@Load 0.100 kg
25.0 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Clear/Translucent
Mix Ratio100:25Volume
 100:25Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO025 / 317084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.