MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Excel Industries EXHALS™ 481 Light Stabilizers
Categories: Other Engineering Material

Material Notes: Regular exposure to heat and light inevitably degrades plastics. Weathering manifests as change in colour emergence of cracks and also diminishes the physical properties of Plastics. Excel Industries Ltd. has introduced EXHALSTM 481 which protects the polymer, helping it withstand ultra violet radiation.

Advantages:

  • Available in powder form (EXHALSTM 481P) or flakes (EXHALSTM 481F) depending on your requirement.
  • Suitable for demanding applications like weather resistance including continued UV exposure for polymers such as PP, HDPE, PS, ABS, SAN, EPDM and PU. It is also effective in PA and POM.
  • Effective independent of the article dimensions, especially for applications with high specific surface area e.g. coating, films, sheets and tapes.

    Information provided by Excel Industries Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.10 %<= 0.10 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 81.0 - 85.0 °C178 - 185 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 99 %
@Wavelength 425 - 450 nm
99 %
@Wavelength 425 - 450 nm
 
Descriptive Properties
Physical stateWhite Powder/Flakes
Purity>99%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Accutech Polyethylene HD0234G30UVL High Density Glass Reinforced UV Stabilized
Tipco Tipcolite® TMHS 291 Phenolic Compound, Khaki Cotton Fabric, in fluffy form, Soft Flow & High Impact Strength
Ethylene Propylene Rubber (EPM, EPDM)
Avient Maxxam™ DP 9052-3-1000 Polyethylene, High Density (HDPE)
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled

PEXCEL025 / 183501

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.