Description: NBR 6240 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6240 is a non staining, medium low mooney, and medium high acrylonitrile polymer designed to aid in processing operations such as extruding and calendaring. NBR 6240 is a low temperature polymerized polymer, and such as, retains the excellent physical and processing properties of a cold nitrile rubber. Applications: NBR 6240 is recommended to use in packings, shoe products, chemically blown sponge, oil field products, industrial and automotive molded parts. CAS No: 9003-18-3 Information provided by LG Chemical |