MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Star Plastics PC20NBR Molding Grade PC with Release  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Information provided by Star Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Maximum Moisture Content 0.0200.020
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
20 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 57.2 MPa8300 psiASTM D638
Tensile Modulus 2.34 GPa340 ksiASTM D638
Flexural Yield Strength 82.7 MPa12000 psiASTM D790
Flexural Modulus 2.34 GPa340 ksiASTM D790
Izod Impact, Notched NBNB73°F, 0.125 in.; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C260 °Funannealed, .125in; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 246 - 274 °C475 - 525 °F
Middle Barrel Temperature 260 - 288 °C500 - 550 °F
Front Barrel Temperature 274 - 302 °C525 - 575 °F
Nozzle Temperature 274 - 302 °C525 - 575 °F
Melt Temperature 274 - 302 °C525 - 575 °F
Mold Temperature 71.1 - 98.9 °C160 - 210 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Back Pressure 0.345 - 1.38 MPa50.0 - 200 psi
Screw Speed 40 - 100 rpm40 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vandar® 8000 PBT, Unfilled
Celanese Vandar® 2500 PBT, Unfilled
Trinseo CALIBRE™ 2061 HD 15 Polycarbonate Resin
Trinseo CALIBRE™ 200-3 Polycarbonate Resin
Covestro Texin® 4215 Thermoplastic Polyurethanes (TPU)

PSTARP18 / 68582

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.