MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sika SikaBond® T35 Trowel-applied, Polyurethane Wood Flooring Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: SikaBond-T35 is a one-component, low-VOC, low odor, moisture cured polyurethane adhesive for full surface bonding of wood flooring. SikaBond-T35 will tenaciously bond wood to most surfaces, including concrete, plywood, and leveling and patch underlayments that have been properly prepared.

Where to Use: SikaBond-T35 may be used to bond all engineered, solid plank flat milled, shorts up to max. 3/4” thick, including bamboo, cork and parquet hardwood flooring designed by the manufacturer for glue down applications. This adhesive can also be used for many other bonding applications that are common for light commercial and residential applications including acoustic rubber underlayment systems.

Advantages:

  • 170% Elongation
  • Low odor
  • Easy to trowel
  • Excellent workability
  • Fast curing
  • Crack bridging
  • Suitable for common types of wood floors
  • Suitable for in-floor radiant heat installation
  • Contains no water
  • Tenacious bond

Information provided by Sika Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Volatile Organic Compounds (VOC) Content <= 60 g/l<= 60 g/l
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050after 28 days
Tensile Strength 1.03 MPa150 psi
Elongation at Break 170 %170 %50% RH
Shear Strength 1.03 MPa150 psi1 mm adhesive thickness at 73°F (23°C) and 50% RH
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min0.750 - 1.00 hour50% RH, Skinning/Laying time
 360 - 480 min6.00 - 8.00 hourFloor may accept light foot traffic depending on climatic conditions and adhesive layer thickness
 1440 min
@Thickness 4.00 mm,
Temperature 23.0 °C
24.0 hour
@Thickness 0.157 in,
Temperature 73.4 °F
50% RH
Shelf Life 12.0 Month
@Temperature 10.0 - 25.0 °C
12.0 Month
@Temperature 50.0 - 77.0 °F
in original unopened cartridge
 
Descriptive Properties
Chemical Base1-component polyurethanemoisture curing
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSIKA921 / 209828

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.