MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper, UNS C19210, H01 Temper sheet
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent soldering, brazing, and coated metal arc welding. Good butt, resistance, and oxyacetylene welding. Gas-shielded arc, spot, and seam resistance welding are not recommended.

Applications: Air conditioner and heat exchanger tubing, lead frames, electrical connectors and terminals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 330 MPa
Elongation at Break 13 %
Modulus of Elasticity 125 GPa
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000216 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.9 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Melting Point <= 1082 °C
Liquidus 1082 °C
Annealing Point 840 - 1020 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 450 - 550 °C
Hot-Working Temperature 700 - 900 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.87 %
Iron, Fe 0.050 - 0.15 %
Phosphorus, P 0.025 - 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 19210 XP-10 Copper Iron, Annealed
Eagle Brass 19210 XP-10 Copper Iron, Hard
Copper, UNS C19210, H02 Temper sheet
Copper, UNS C19210, H04 Temper sheet
Eagle Brass 19210 XP-10 Copper Iron, Spring

MC19210b1 / 10938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.