MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Purell 2410T Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: Purell 2410T is low-density polyethylene grade with a good combination of flowability and softness. The grade is used for all types of injection molded applications in the healthcare market. Applications: Caps & Closures (Healthcare), Healthcare Applications, Medical Devices

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccISO 1183-1
Environmental Stress Crack Resistance 0.50 hour
Melt Flow 36 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 49ISO 868
Ball Indentation Hardness 18.0 MPaISO 2039-1
Tensile Strength, Yield 11.0 MPaISO 527-1,-2
Tensile Modulus 280 MPaISO 527-1,-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 112 °CDSC; ISO 3146
Vicat Softening Point 89.0 °CA50N; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)H 49/30
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin
Chevron Phillips Marlex® K203 LLDPE Sheet Extrusion
Dow 959S Linear Low Density Polyethylene (LDPE)
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin
ExxonMobil LL 5100.09 LLDPE Master Batch Resin

PEQT8614 / 220248

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.