MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler

Material Notes: Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on metal and EPOXIDUR EP 3581 T-1 part surfaces. Sensor encapsulation in the automobile industry. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection and compression molding

Information provided by Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.93 - 1.98 g/ccISO 1183
Apparent Bulk Density 0.0800 - 0.0900 g/ccISO 60
Water Absorption <= 0.10 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmInjection and Compression; ISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 70.0 - 90.0 MPaInjection and Compression; ISO 527
Modulus of Elasticity 15.0 - 18.0 GPaInjection and Compression; ISO 527
Flexural Strength 140 - 160 MPaInjection and Compression; ISO 178
Flexural Modulus 15.0 - 20.0 GPaInjection and Compression; ISO 178
Compressive Strength 200 - 250 MPaISO 604
Charpy Impact Unnotched 12.0 - 14.0 kJ/m²Injection and Compression; ISO 179/1eU
Charpy Impact, Notched 2.00 - 4.00 kJ/m²Injection and Compression; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 - 1.00e+14 ohmIEC 60093
Dielectric Constant 4.0 - 6.0
@Frequency 1e+6 Hz
IEC 60250
 5.0 - 7.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 25.0 - 35.0 kV/mmIEC 60243-1
Dissipation Factor 0.010 - 0.030
@Frequency 1e+6 Hz
IEC 60250
 0.030 - 0.050
@Frequency 100 Hz
IEC 60250
Arc Resistance 180 - 240 secASTM D495
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 50.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.400 - 0.600 W/m-KASTM E1461
Maximum Service Temperature, Air 180 °C
@Time 7.20e+7 sec
IEC 60216/T1
 250 °C
@Time <=180000 sec
IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-A
Deflection Temperature at 8.0 MPa 160 - 180 °CISO 75-C
Flammability, UL94 HB
@Thickness 1.60 mm
Shrinkage <= 0.050 %
@Temperature 110 °C,
Time 605000 sec
Post shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature <=15.0 °C
 
Descriptive Properties
Glow wire flammability test900/1IEC 60695 2-12
Glow wire ignitability test900/1IEC 60695 2-13
Water Absorption<10 mg24 hr, 23°C; ISO 62

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Molded, Glass Fiber Filler
Hexcel® HexFlow® RTM 6 180°C Epoxy System for Resin Transfer Molding Monocomponent System
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy

PRASCI05 / 179142

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.