MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Hot-Rolled
Categories: Metal; Nonferrous Metal; Zinc Alloy

Material Notes: Hot Work Temperature 175-300°C

Properties vary with rolling direction. Values for longitudinal and transverse directions are listed separately.

Key Words: UNS Z44330
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.17 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 52500 kg load; 10 mm hardened steel ball
Hardness, Vickers 67Estimated from Brinell Value
Tensile Strength, Ultimate 170 - 210 MPa
Elongation at Break 35 - 50 %
Fatigue Strength 28.0 MPa
@# of Cycles 1.00e+8
rotating beam
Shear Strength 138 - 152 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000620 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.1 - 34.7 µm/m-°C
@Temperature 20.0 - 40.0 °C
Specific Heat Capacity 0.402 J/g-°C
Thermal Conductivity 104.7 W/m-K
Melting Point 419 - 422 °C
Solidus 419 °C
Liquidus 422 °C
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 175 - 300 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0010 %
Cadmium, Cd <= 0.0050 %
Copper, Cu 0.85 - 1.25 %
Iron, Fe <= 0.012 %
Lead, Pb <= 0.10 %
Tin, Sn <= 0.0010 %
Zinc, Zn 98.631 - 99.15 %As balance; per ASTM B 69

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper-Hardened Rolled Zinc (Zn-1.0Cu), Cold-Rolled
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Cold-Rolled
Commercial Rolled Zinc (Zn-0.06Pb-0.06Cd), Hot-Rolled
Overview of materials for Zinc Alloy
Commercial Rolled Zinc (Zn-0.08Pb), Hot-Rolled

MZN754 / 14564

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.