Diene™55AC10 is a solution polymerized plastics grade medium cis polybutadiene, featuring excellent color and low gel. It is intermediate in solution viscosity and contains a non-volatile antioxidant system. Diene™55AC10 is widely used as an impact modifier for thermoplastic resins such as HIPS and ABS.Information provided by Lion Elastomer |