MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 241-73W236 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains a stabilization system for protection against copper and other metal-catalyzed degradation. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • Complies with NSF Standard 61: Piping System Components for Drinking Water.
  • Compliant to EU Directive 2003/11/EC regarding marketing and use of certain dangerous substances and preparations, specifically pentabromodiphenyl ether or octabromodiphenyl ether.
  • EU and China RoHS compliant.
Applications:
  • Plumbing – Potable Water Seals and Gaskets
  • Tubing
Uses:
  • Plumbing Parts
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemcial

Key Words: EU 2003/11/EC; NSF 51; NSF 61; RoHS Compliant; UL QMFZ2; UL QMFZ8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.970 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 792 mm, 15 sec; ISO 868
Tensile Strength at Break 1280 psiAcross Flow; ASTM D412
Tensile Stress at Strain 522 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 490 %Across Flow; ASTM D412
Compression Set 25 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 57 %
@Temperature 100 °C,
Time 605000 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
Rear Barrel Temperature 350 °F
Middle Barrel Temperature 360 °F
Front Barrel Temperature 370 °F
Nozzle Temperature 380 - 440 °F
Die Temperature 400 °FExtrusion
Melt Temperature 395 °FExtrusion
 390 - 450 °FProcessing
Mold Temperature 50.0 - 125 °FProcessing
Drying Temperature 180 °F
Dry Time 3 hour
Moisture Content 0.080 %
Back Pressure 50.0 - 100 psiProcessing
 725 - 2900 psiExtrusion
Clamp Pressure 6000 - 10000 psi
Vent Depth 0.00100 in
Cushion 0.125 - 0.250 in
Screw Speed 100 - 200 rpm
 
Descriptive Properties
ColorNatural Color
FormPellets
Injection RateFast
Maximum Regrind %20
Screw Compression Ratio2:1 - 2.5:1
Screw L/D Ratio16:1 - 20:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom ERG 393F BLACK Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F C1 BLACK Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F C12509 Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F NA BLACK Polypropylene with 20% Glass Fiber Filler
Asahi Kasei Thermylene® P6-10FG-Y950 10% Glass Fiber Reinforced, Lubricated Polypropylene

PADVA117 / 22807

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.