MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

KaMin KaMin® Tek 2001 Clay
Categories: Ceramic; Clay

Material Notes: The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect on gloss.

Industry: Paint & Coatings

Uses: Architectural Coatings, Industrial Coatings, Wood Coatings, Satin, Gloss

Information provided by KaMin LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.60 g/cc2.60 g/cc
Bulk Density 0.801 - 0.897 g/cc0.0289 - 0.0324 lb/in³Loose
Solids Content 69.5 - 71 %69.5 - 71 %Slurry
Brightness 91 - 92.5 %91 - 92.5 %Reflectance (TAPPI)
Oil Absorption 34 %34 %
Fineness >= 5>= 5Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %<= 1.5 %As Produced
Particle Size 0.25 µm0.25 µmAverage Stokes Equivalent Diameter
 0.62 µm0.62 µmMedian (Malvern Laser)
Particle Mesh Size 325 Mesh325 Mesh0.005% Retained
pH 6 - 86 - 8100 g/250 ml H2O Slurry
Specific Surface Area 20 m²/g20 m²/gBET
Brookfield Viscosity 500 cP
@Temperature 25.0 °C
500 cP
@Temperature 77.0 °F
20 RPM
 
Descriptive Properties
Bulking Value21.7 lb.gal
CAS Number1332-58-7
Crystalline Silica (quartz)<0.1%
Physical FormsDry, Slurry
Shipping PointWrens, GA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CKAMAN924 / 178395

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.