LORD Circalok™ 6756 primer is designed for use in electronics applications to bond Room Temperature Vulcanized (RTV) silicone rubbers to most metals and glass. It may also be used to bond addition-cure RTV silicones. Circalok 6756 primer is flammable. Do not store or use near heat, sparks or open flame. Features: provides good adhesion on most RTV silicone rubbers, as well as addition-cure RTV systems. provides superior hydrolytic stability. All information provided by Lord. |