MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Duratron® D7015G PI Bearing Grade Polyimide (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Water Absorption 0.50 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 3.0 %ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 126ASTM D785
Hardness, Shore D 87ASTM D2240
Tensile Strength 11000 psiASTM D638
Tensile Strength at 150°C (300°F) 9000 psiASTM D638
Tensile Strength at 65°C (150°F) 11000 psiASTM D638
Elongation at Break 3.0 %ASTM D638
Tensile Modulus 650 ksiASTM D638
Flexural Strength 16500 psiASTM D790
Flexural Modulus 640 ksiASTM D790
Compressive Strength 25000 psi10% Deformation; ASTM D695
Compressive Modulus 360000 psiASTM D695
Shear Strength 13000 psiASTM D732
Izod Impact, Notched 0.800 ft-lb/inASTM 256 Type 'A'
Coefficient of Friction, Dynamic 0.25Dry vs. Steel; QTM 55007
K (wear) Factor 10.0 x 10-10 in³-min/ft-lb-hrQTM55010
Limiting Pressure Velocity 40000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 10000 ohmEOS/ESD S11.11
Dielectric Constant 5.42
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 186 kV/inASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 21.5 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Thermal Conductivity 2.70 BTU-in/hr-ft²-°FASTM E1530
Melting Point 580 °F
Maximum Service Temperature, Air 500 °FContinuous
Deflection Temperature at 1.8 MPa (264 psi) 690 °FASTM D648
Glass Transition Temp, Tg 660 °FASTM D3418
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Acceptable
Conductive / Static Dissipative Yes
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Duratron® D7000 PI Unfilled Polyimide (ASTM Product Data Sheet)
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
DuPont Mobility and Materials Vespel® SP-21 Polyimide, 15% Graphite Filled, Direct formed
Mitsubishi Chemical Advanced Materials Duratron® CU60 PBI Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)
KEP Kepital® F10-03H Acetal Copolymer, High viscosity, High rigidity

P1SM05u / 104385

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.