MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Veradel® 3300 SL30 Polyethersulfone (PESU)
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Veradel® 3300 SL30 is a polyethersulfone (PESU) compound designed to provide a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and externally lubricated applications. The resin is formulated with a ternary anti-friction/anti-wear additive system comprised of carbon fiber, graphite, and polytetrafluoroethylene (PTFE).

Veradel® PESU is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, ease of melt processing, high purity, and excellent chemical resistance.

These properties make it well-suited for applications in transportation, electronics, chemical processing, and industrial uses. The resin is black in color in its natural state.

Applications: Automotive Applications; Bearings; Bushings; Gears; Industrial Applications; Profiles; Rods; Sheet

Features: Chemical Resistant; Good Dimensional Stability; High Heat Resistance; Low Friction; Medium Flow; Wear Resistant

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.53 g/cc0.0553 lb/in³ASTM D792
Water Absorption 0.31 %
@Time 86400 sec
0.31 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0017 cm/cm0.0017 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 380 °C
9.0 g/10 min
@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7676ISO 2039-2
Hardness, Rockwell R 115115ISO 2039-2
Tensile Strength, Yield 130 MPa18900 psiType 1A, 5 mm/min; ISO 527-2
Elongation at Break 1.6 %1.6 %ASTM D638
Tensile Modulus 12.0 GPa1740 ksi1 mm/min, Type 1A; ISO 527-2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 12.0 GPa1740 ksiISO 178
Compressive Strength 165 MPa23900 psiISO 604
Compressive Modulus 12.2 GPa1770 ksiISO 604
Shear Strength 62.1 MPa9010 psiASTM D732
Izod Impact, Notched (ISO) 8.00 kJ/m²3.81 ft-lb/in²ISO 180
Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 62000 ohm-cm62000 ohm-cmASTM D257
Surface Resistance 20000 ohm20000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 0.000 - 180 °C
5.56 µin/in-°F
@Temperature 32.0 - 356 °F
ASTM D696
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Glass Transition Temp, Tg 220 °C428 °FDSC
 
Processing PropertiesMetricEnglishComments
Melt Temperature 340 - 385 °C644 - 725 °FInjection
Mold Temperature 130 - 170 °C266 - 338 °F
Drying Temperature 177 °C
@Time 9000 sec
351 °F
@Time 2.50 hour
 
Descriptive Properties
AdditiveCarbon Fiber + Graphite + PTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4592 / 280392

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.