Product Description: A is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Low sealing threshold
- High seal strength even under low pressure
- Good aroma barrier
- Excellent packaging machine performances
- Outstanding optical properties
- Excellent stiffness
- Ideal support for normal ink systems
- Water-based coatings
Features:- Acrylic Coated
- Flavor & Aroma Barrier
Applications:- Biscuits/Cookie/Crackers
- Box Overwrap
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Health and Beauty Care
- Household and Detergents
- Pet Food
Uses: - Box Overwrap Flexible Packaging
- HFFS Flexible Packaging
- Pre-made – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Solvent Flexographic Printing, Solvent Rotogravure Printing and Surface Print UnsupportedInformation provided by ExxonMobil |