MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV 24464 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink 24464 is a general purpose thermoplastic vulcanizate used in automotive and industrial applications. This product is a medium hardness, low density, RoHS compliant grade suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Low Density; Low Flow; Low Specific Gravity; Lubricated; Medium Hardness; Slip

Uses: Expansion Joint; Gaskets; Glazing: Grommets; Plugs; Shock Absorbing Pads; Tubing; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ISO 1183
Viscosity 164 cP
@Shear Rate 206 1/s,
Temperature 200 °C
164 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  65
@Time 15.0 sec
65
@Time 0.00417 hour
Injection Molded; ISO 868
 66
@Time 5.00 sec
66
@Time 0.00139 hour
Injection Molded; ISO 868
 69
@Time 1.00 sec
69
@Time 0.000278 hour
Injection Molded; ISO 868
 66.5
@Treatment Temp. 125 °C,
Time 15.0 sec
66.5
@Treatment Temp. 257 °F,
Time 0.00417 hour
Injection Molded, Change in Air, 168; ISO 888
 67.1
@Treatment Temp. 125 °C,
Time 5.00 sec
67.1
@Treatment Temp. 257 °F,
Time 0.00139 hour
Injection Molded, Change in Air, 168; ISO 888
 67.5
@Treatment Temp. 110 °C,
Time 15.0 sec
67.5
@Treatment Temp. 230 °F,
Time 0.00417 hour
Injection Molded, Change in Air, 1008; ISO 888
 68.1
@Treatment Temp. 110 °C,
Time 5.00 sec
68.1
@Treatment Temp. 230 °F,
Time 0.00139 hour
Injection Molded, Change in Air, 1008; ISO 888
 69.9
@Treatment Temp. 125 °C,
Time 1.00 sec
69.9
@Treatment Temp. 257 °F,
Time 0.000278 hour
Injection Molded, Change in Air, 168; ISO 888
 71
@Treatment Temp. 110 °C,
Time 1.00 sec
71
@Treatment Temp. 230 °F,
Time 0.000278 hour
Injection Molded, Change in Air, 1008; ISO 888
Tensile Strength at Break 3.66 MPa531 psiAcross Flow, Type 1, 20 in/min; ISO 37
 4.36 MPa632 psiFlow, Type 1, 20 in/min; ISO 37
 3.76 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
545 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
 3.84 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
557 psi
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 4.21 MPa
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
611 psi
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 4.29 MPa
@Treatment Temp. 125 °C,
Time 605000 sec
622 psi
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain  2.03 MPa
@Strain 100 %
295 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 3.45 MPa
@Strain 100 %
500 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 2.17 MPa
@Strain 100 %,
Treatment Temp. 110 °C
314 psi
@Strain 100 %,
Treatment Temp. 230 °F
Across Flow, Type 1, Change in Air in 1008 hr; ISO 188
 2.21 MPa
@Strain 100 %,
Treatment Temp. 125 °C
320 psi
@Strain 100 %,
Treatment Temp. 257 °F
Across Flow, Type 1, Change in Air in 168 hr; ISO 188
 3.76 MPa
@Strain 100 %,
Treatment Temp. 110 °C
545 psi
@Strain 100 %,
Treatment Temp. 230 °F
Flow, Type 1, Change in Air in 1008 hr; ISO 188
 3.79 MPa
@Strain 100 %,
Treatment Temp. 125 °C
550 psi
@Strain 100 %,
Treatment Temp. 257 °F
Flow, Type 1, Change in Air in 168 hr; ISO 188
Elongation at Break 210 %210 %Flow, Type 1, 20 in/min; ISO 37
 290 %290 %Across Flow, Type 1, 20 in/min; ISO 37
 162 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
162 %
@Treatment Temp. 230 °F,
Time 1008 hour
Flow, Type 1, Change in Air; ISO 188
 162 %
@Treatment Temp. 125 °C,
Time 605000 sec
162 %
@Treatment Temp. 257 °F,
Time 168 hour
Flow, Type 1, Change in Air; ISO 188
 275 %
@Treatment Temp. 125 °C,
Time 605000 sec
275 %
@Treatment Temp. 257 °F,
Time 168 hour
Across Flow, Type 1, Change in Air; ISO 188
 282 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
282 %
@Treatment Temp. 230 °F,
Time 1008 hour
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 15.1 kN/m86.0 pliMethod Ba, Angle (Unnicked), Across Flow, 20 in/min; ISO 34-1
 16.8 kN/m96.0 pliMethod Ba, Angle (Unnicked), Flow, 20 in/min; ISO 34-1
Compression Set  17 %
@Temperature 22.8 °C,
Time 79200 sec
17 %
@Temperature 73.0 °F,
Time 22.0 hour
Type A; ISO 815
 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
Type A; ISO 815
 31 %
@Temperature 90.0 °C,
Time 252000 sec
31 %
@Temperature 194 °F,
Time 70.0 hour
Type A; ISO 815
 46 %
@Temperature 125 °C,
Time 252000 sec
46 %
@Temperature 257 °F,
Time 70.0 hour
Type A; ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 230 °C374 - 446 °FInjection, Melt
Rear Barrel Temperature 173 - 213 °C344 - 416 °FInjection
Middle Barrel Temperature 179 - 219 °C354 - 426 °FInjection
Front Barrel Temperature 184 - 224 °C364 - 436 °FInjection
Nozzle Temperature 190 - 230 °C374 - 446 °FInjection
Zone 1 166 - 204 °C330 - 400 °FExtrusion
Zone 2 171 - 210 °C340 - 410 °FExtrusion
Zone 3 177 - 216 °C350 - 420 °FExtrusion
Zone 4 180 - 219 °C356 - 426 °FExtrusion
Zone 5 182 - 221 °C360 - 430 °FExtrusion
Die Temperature 190 - 227 °C374 - 440 °FExtrusion
Mold Temperature 35.0 - 60.0 °C95.0 - 140 °FInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1188 / 237679

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.