MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PSM Industries Pacific Sintered Metals FX-227-T Infiltrated Steel Powdered Metal (MPIF FX-1005-50)
Categories: Metal; Ferrous Metal

Material Notes: Machines and plates well. Good in hydraulic applications. Moderate tolerance control.

Equivalent MPIF Specification: FX-1005-50

All information provided by Pacific Sintered Metals.

Key Words: PM
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.20 - 7.50 g/cc0.260 - 0.271 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8282
Tensile Strength, Ultimate 531 MPa77000 psi
Tensile Strength, Yield 345 MPa50000 psi
Elongation at Break 4.0 %4.0 %
Modulus of Elasticity 110 GPa16000 ksi
Flexural Strength 1090 MPa158000 psiTransverse Rupture
Charpy Impact, Unnotched 17.6 J13.0 ft-lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zircar Zirconia ZOF-100 Pure Zirconia Felt Insulation
Special Metals MONEL® Alloy 400
Silicon Carbide, Alpha SiC
SGL Carbon Group SIGRAFIL C® C30 T045 EPY Continuous Tow Carbon Fiber with 45k filaments, Epoxy Sizing
Sapco Silicon Nitride, Si3N4

NPACIF026 / 86184

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.