Same nominal composition but higher Si and Fe impurity limits than Al-5657 Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN. Composition Notes: Composition information provided by the Aluminum Association and is not for design. |
UNS A95005; ISO AlMg1; Aluminium 5005-O; AA5005-O; Al5005-O |