Lupolen 2421 F is an additivated, low density polyethylene. It is characterized by a good melt strength leading to a good bubble stability during blown film extrusion. It contains an antioxidant and is delivered in pellet form. This product is not intended for use in medical and pharmaceutical applications. Applications: Agriculture Film, Bags & Pouches, Food Packaging Film, Hygiene Film, Liner Film, Shrink FilmInformation provided by LyondellBasell. |