MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Morgan Advanced Ceramics P-3 Ceramic Core Material Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: High silica core type with intermediate particle size distribution and excellent high temperature stability. Used for DS and SX applications where there are blind passages and core leachability is a concern

Information provided by Morgan Advanced Materials

Key Words: P-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.60 g/cc0.0578 lb/in³
Density 2.30 g/cc0.0831 lb/in³
Water Absorption >= 20 %>= 20 %
Open Porosity 32 %32 %
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00862 GPa1.25 ksi4 point
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.40 µm/m-°C
@Temperature 25.0 - 1000 °C
1.33 µin/in-°F
@Temperature 77.0 - 1830 °F
Shrinkage 0.90 %0.90 %chord, mold to fired
 1.1 %1.1 %length, mold-to-fired
 
Component Elements PropertiesMetricEnglishComments
Al2O3 3.0 %3.0 %
Antimony, Sb >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Bismuth, Bi >= 0.00010 %>= 0.00010 %trace element, 1 ppm
Iron, Fe >= 0.090 %>= 0.090 %trace element, 900 ppm
Lead, Pb >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Other >= 1.0 %>= 1.0 %
 3.0 %3.0 %ZrSiO4
Silver, Ag >= 0.0025 %>= 0.0025 %trace element, 25 ppm
SiO2 93 %93 %
Tin, Sn >= 0.0025 %>= 0.0025 %trace element, 25 ppm
Zinc, Zn >= 0.0050 %>= 0.0050 %trace element, 50 ppm
 
Descriptive Properties
Cristobalite Content14 percent, after fire
 63 percent after 30 min at 1530°C
Leachability100 percent, 30 percent boiling KOH, 30 g sample, 15 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF5097 / 200334

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.