MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 6 FRM1X3 PA6, flame retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Features

Determined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material predetermines it for the manufacturing of complicated small and large surface mouldings. Possible use for products with wall thickness from 0.5 mm. High grade brightness also at coloured types. Delivered in the full RAL colour scale.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PA6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³
Viscosity Measurement 1.11 - 1.151.11 - 1.15
Linear Mold Shrinkage 0.0115 cm/cm0.0115 in/in
Linear Mold Shrinkage, Transverse 0.0111 cm/cm0.0111 in/in
Melt Flow 10 g/10 min
@Load 0.325 kg,
Temperature 270 °C
10 g/10 min
@Load 0.716 lb,
Temperature 518 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi
Elongation at Break 3.5 %3.5 %
Tensile Modulus 3.20 GPa464 ksi
Flexural Strength 105 MPa15200 psi
Flexural Modulus 2.70 GPa392 ksi
Charpy Impact Unnotched  11.0 J/cm²
@Temperature -20.0 °C
52.3 ft-lb/in²
@Temperature -4.00 °F
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Charpy Impact, Notched  0.200 J/cm²
@Temperature 23.0 °C
0.952 ft-lb/in²
@Temperature 73.4 °F
 0.200 J/cm²
@Temperature -20.0 °C
0.952 ft-lb/in²
@Temperature -4.00 °F
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
Surface Resistance 1.00e+12 ohm1.00e+12 ohm
Dielectric Strength 20.0 kV/mm508 kV/in
Comparative Tracking Index 500 V500 V
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °F
Vicat Softening Point 200 °C392 °FB
Flammability, UL94 V-0V-0
Glow Wire Test 960 °C1760 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 50.0 - 70.0 °C122 - 158 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACO356 / 120980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.