MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resinlab® CA5015 Cyanoacrylate Adhesive
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: ResinLab® CA5015 is a one part, high viscosity, odorless moisture cure cyanoacrylate. It has been formulated to have low blooming, non irritating and non staining characteristics. CA5015 bonds well to various substrates such as metals, plastics and elastomers as well as porous or absorbent materials like wood, paper, leather and textiles. CA5015 is well suited for applications where vapor control is difficult. Surface moisture will initiate the hardening process. Handling strength is reached quickly and can vary depending on environmental conditions and type of substrate used. This product will continue to cure for at least 24 hours before full strength and chemical resistance is achieved. Allow product to develop full strength before use with full loads. CA5015 is suitable for use in medical device assembly. It has been tested and is proven non-toxic per ISO 10993-5. Manufacturers should test their own finished product for biocompatibility.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Brookfield Viscosity 735 - 775 cP735 - 775 cP#21 spindle@50 rpm
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 3.00 - 5.00 MPa435 - 725 psiLap Shear, Cured for 24 hours @ 22°C, Aluminum; ISO 4587
 6.998 - 8.96 MPa1015 - 1300 psiLap Shear, substrate failure, Cured for 24 hours @ 22°C, Polycarbonate; ISO 4587
 10.0 - 13.00 MPa1450 - 1885 psiLap Shear, substrate failure, Cured for 24 hours @ 22°C, ABS; ISO 4587
 10.0 - 14.0 MPa1450 - 2030 psiLap Shear, Cured for 24 hours @ 22°C, Steel; ISO 4587
 13.00 - 14.5 MPa1885 - 2100 psiLap Shear, substrate failure, Cured for 24 hours @ 22°C, Beech Wood; ISO 4587
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull cure, ABS
 1440 min24.0 hourFull cure, Polycarbonate
 1440 min24.0 hourFull cure, Aluminum
 1440 min24.0 hourFull cure, Steel
 1440 min24.0 hourFull cure, Beech Wood
Pot Life 0.0833 - 0.250 min0.0833 - 0.250 minFixture time, Steel
 0.0833 - 0.250 min0.0833 - 0.250 minFixture time, Beech Wood
 0.167 - 0.333 min0.167 - 0.333 minFixture time, Aluminum
 0.250 - 0.500 min0.250 - 0.500 minFixture time, ABS
 0.333 - 0.500 min0.333 - 0.500 minFixture time, Polycarbonate
Shelf Life 12.0 Month
@Temperature 2.00 - 8.00 °C
12.0 Month
@Temperature 35.6 - 46.4 °F
 
Descriptive Properties
ColorTransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESL202 / 248990

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.