MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool® VF Shapes and Boards Plus Strong VF Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® Plus™ Strong VF is produced by the addition of selected refractory fillers in order to maximize the mechanical properties and the resistance to erosion of the final product.

Typical applications:

  • Riser sleeves and crucibles for ferrous and non ferrous molten metals
  • Stopper nut insulation
  • Ladle shroud gasket
  • Nozzle insulation in continuous casting
  • Roller inserts in roller hearth furnace
  • Glass casting mould
  • Tube insulation end in tube fumes boiler
  • Insulation for domestic appliance
  • Furnace insulation

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.380 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000900 GPafired
 0.00201 GPaunfired
Compressive Strength 0.300 MPaat 5% compression
 0.380 MPaat 10% compression
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0900 W/m-K
@Temperature 400 °C
ASTM C-201
 0.120 W/m-K
@Temperature 600 °C
ASTM C-201
 0.140 W/m-K
@Temperature 800 °C
ASTM C-201
 0.170 W/m-K
@Temperature 1000 °C
ASTM C-201
Shrinkage <= 2.0 %
@Temperature 1100 °C,
Time 86400 sec
isothermal, permanent
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 5.0 - 7.0 %
 
Descriptive Properties
Classification Temperature (°C)1200
Colorwhite/tan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF7017 / 203316

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.