MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite Durez® 10694 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: DUREZ 10694 is a one step liquid based on phenolic resol (TS) polymer. It is supplied in the form of liquid for adhesives. It is recommended for use in adhesive applications.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccDCT 5075
Volatiles 21 %21 %DCT 4005A
Water Absorption 50 %50 %DCT 4012A
pH 7.07.0DCT 4064A
Viscosity Measurement 4545G&H; DCT 4003A
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58DCT 0005
 
Processing PropertiesMetricEnglishComments
Cure Time 0.758 min
@Treatment Temp. 165 °C
0.0126 hour
@Treatment Temp. 329 °F
DCT 4001D

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32025 Phenolc Resin
Sumitomo Bakelite Durez® P23056NF Phenolic Resin
Sumitomo Bakelite Durez® 32025B Phenolic Resin
Sumitomo Bakelite Durez® 12687 CNSL Phenolic Resin
Sumitomo Bakelite Durez® 118 Phenolic, Injection Grade

PSUMIT210 / 194015

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.