MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Esstech X-950-0000 BisGMA Resin, C29H36O8
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Bisphenol A Glycidyl Methacrylate or bis-GMA is a high viscosity resin that has been used in dental formulations for years. Our BisGMA is manufactured with low levels of BPA or bisphenol A and low color. Listed on the Toxic Substance Control Act List. CAS # 1565-94-2.

Information provided by ESSTECH, Inc.

Key Words: C29H36O8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 700000 cP700000 cP
Molecular Weight 512.599 g/mol512.599 g/mol
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54
 
Descriptive Properties
Acidity (KOH per g)4.2 mg
Color (APHA)< 50
HQ Inhibitor (ppm)< 350
MeHQ Inhibitor (ppm)< 600
Purity (%)> 85

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Corning Gorilla® Glass 6 Display Glass
Esstech V-117-1095 Barium Borosilicate Glass
Esstech V-117-1190 Barium Borosilicate Glass
Esstech V-117-1112 Barium Borosilicate Glass
Esstech V-117-1075 Barium Borosilicate Glass

PESST028 / 108299

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.