System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Flint Hills P5C6Z-075 Random Copolymer Polypropylene
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene, Fiber Grade
Material Notes:
Features:
Phthalate-free.
Applications:
Fibers, BCF, Spunbonded
Information provided by Flint Hills Resources.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.900
g/cc
ASTM D1505
Melt Flow
38
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
93
ASTM D785
Tensile Strength, Yield
30.0
MPa
ASTM D638
Elongation at Yield
13 %
ASTM D638
Flexural Modulus
1.096
GPa
Tangent; ASTM D790
Flexural Modulus, 1% Secant
1027
MPa
ASTM D790
Izod Impact, Notched
27.0
J/m
ASTM D256
Gardner Impact
2.00
J
ASTM D5420
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
93.0
°C
ASTM D648
Compliance Properties
Original Value
Comments
FDA
Yes
21 CFR 177.1520(c) 3.2a
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Flint Hills AP5995-HA Polypropylene Impact Copolymer
Flint Hills P4C5B-075 Homopolymer Polypropylene
Flint Hills P5M5R-083 Random Copolymer Polypropylene
Flint Hills P5M6K-101X Random Copolymer Polypropylene
Flint Hills 23T2A Random Copolymer Polypropylene
PFLINT818 / 142630
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.