MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Outokumpu 4742 High Temperature Ferritic Stainless Steel
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form after long time exposures to temperatures around 650°C.

Applications: Mostly used in high temperature applications with sulphurous atmospheres and/or low tensile loads such as for installations within:

  • Chemical industry (drums)
  • Power industry (coal burners)
  • Metalworking industry (heat treatment boxes)
  • Furnace technology (walls, doors)

Available in hot rolled plate (Quarto) form.

Key Words: EN 1.4742
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.60 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 212RT; EN 10003-1
Tensile Strength, Ultimate 535 MPaOutokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 375 MPa
@Strain 0.2 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 405 MPa
@Strain 1 %
Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
Elongation at Break 25 %Outokumpu Typical, Hot Rolled Plate (Quarto); EN 10002-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000910 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.1 µm/m-°C
@Temperature 600 °C
 12.9 µm/m-°C
@Temperature 800 °C
Specific Heat Capacity 0.450 J/g-°CRT
Thermal Conductivity 16.0 W/m-KRT
 22.3 W/m-K
@Temperature 500 °C
Maximum Service Temperature, Air 1000 °CDry Air
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 800 - 850 °CCooling: forced air or water
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.70 %
Carbon, C 0.12 %
Chromium, Cr 18 %
Iron, Fe 81.18 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Special Metals INCONEL® Alloy 600
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Universal Wire Works 309 Stainless Steel Electrode
Mo-Sci Corporation GL 1702 Glass-ceramic

NOUTOK38 / 18753

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.