MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e housings, plug-and-socket connectors.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 - 0.900 g/cc0.0217 - 0.0325 lb/in³
Water Absorption 0.40 %0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %0.20 %ISO 62
Viscosity Test 95 cm³/g0.95 dl/gISO 307
Linear Mold Shrinkage, Flow 0.0013 cm/cm0.0013 in/inplate with film gate 150x150x3mm3
 0.0032 cm/cm0.0032 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.00889 cm/cm0.00889 in/inplate with film gate 150x150x3mm3
 0.0097 cm/cm0.0097 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 120 MPa17400 psiISO 527-1/-2
Elongation at Break 2.2 %2.2 %ISO 527-1/-2
Tensile Modulus 9.50 GPa1380 ksiISO 527-1/-2
Charpy Impact Unnotched  4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.780 J/cm²
@Temperature 23.0 °C
3.71 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmIEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.0046
@Frequency 100 Hz
0.0046
@Frequency 100 Hz
IEC 60250
 0.0202
@Frequency 1e+6 Hz
0.0202
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 V425 VTest Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 11357-1/-2
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75-1/-2
Decomposition Temperature >= 300 °C>= 572 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Ignition Temperature >= 400 °C>= 752 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 275 °C482 - 527 °FInjection molding/Extrusion
Mold Temperature 60.0 - 100 °C140 - 212 °FInjection molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT

PBASG0132 / 131765

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.