MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ConocoPhillips Hydroclear® 10 Ultra-Clean Spindle Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties of a light spindle oil and light hydraulic oil are required.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.8506 g/cc0.8506 g/ccASTM D-4052
API Gravity 34.9 °34.9 °ASTM D-1298
Kinematic Viscosity 20.1 cSt
@Temperature 21.0 °C
20.1 cSt
@Temperature 69.8 °F
ASTM D 445
Kinematic Viscosity at 40°C (104°F) 10.04 cSt10.04 cStASTM D 445
Kinematic Viscosity at 100°C (212°F) 2.6 cSt2.6 cStASTM D 445
ASTM Color <= 0.50<= 0.50
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0300.030mg KOH/g; ASTM D-974
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.0290.029ASTM D4172A
Four Ball Wear 0.215 mm0.00846 inScar Diameter; ASTM D-4172A
 
Thermal PropertiesMetricEnglishComments
Pour Point -37.2 °C-35.0 °FASTM D-97
Flash Point 171 °C340 °FASTM D-92
 
Descriptive Properties
Copper Corrosion1AASTM D130
Emulsion Characteristics (40-40-0)10 minutesASTM D-1401
Freshwater Rust TestPassASTM D665A
ISO Cleanliness Code14/11Applies to packaged goods only.
Sim. Seawater Rust TestPassASTM D665B
Thermal Stability4 mg/100 mLMod. CM "A" Sludge

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON140 / 75177

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.