MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® A XP 2770 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Aqueous hydroxyfunctional polyacrylic dispersion, in combination with aliphatic polyisocyanates for waterborne 2K-polyurethane coatings.

Properties / Applications: Bayhydrol® A XP 2770 is a hydroxyfunctional polyacrylic dispersion which can be thinned with water to application viscosity. Bayhydrol® A XP 2770 combined with aliphatic polyisocyanates yields high-gloss top coats which can be dried at room temperature or force-dried, e.g. at 80 °C. The cured paint films are hard and flexible with outstanding resistance to solvents and water and excellent weatherability. When properly formulated, e.g. in combination with Bayhydur® 304 in an NCO / OH ratio of 1.5 : 1, the pot life is approx. 4 hours. Bayhydrol® A XP 2770 has good pigment wetting properties and high shear stability. Bead mills have proved suitable as grinding equipment. Only pigments and extenders with a minimum water-soluble content should be used. Given the many pigments and extenders available, compatibility testing should always be carried out. When mixing Bayhydur® or Desmodur® into the mill base, a thickener must be added to ensure a high shear effect. The addition of approximately 0.4 % Borchigen® PW 25 (calculated on the solid binder) has proved suitable for formulations based on Bayhydrol® A XP 2770. Levelling and substrate wetting can be optimised by adding, for example Byk® 349 and Byk® 378. Byk® 011 has proved to be a suitable antifoam. Application and formulation equipment can be cleaned with water, alkaline cleaning agents or isopropanol.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccDIN EN ISO 2811
Volatiles 54 - 58 %1g/1h/125 °C/convection oven; DIN EN ISO 3251
pH 7.0 - 9.010% in demineralized water; DIN ISO 976
Viscosity 200 - 1200 cPD= approx. 40 s-1; DIN EN ISO 3219/A.3
 
Chemical PropertiesOriginal ValueComments
Acid Value 11[mg KOH/g]; DIN EN ISO 2144
 
Descriptive Properties
Content3.9%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0159 / 201942

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.