MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abatron AboCast 50-11/AboCure 50-1 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Information provided by Abatron, Inc.

Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).

Key Words: potting, casting, encapsulating, impregnating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 2300
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 75
Tensile Strength, Ultimate 54.33 MPa
Elongation at Break 14.4 %
Flexural Yield Strength 78.81 MPa
Flexural Modulus 1.58 GPa
Compressive Yield Strength 71.02 MPa
Compressive Modulus 1.65 GPa
Izod Impact, Notched 0.235 J/cm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.42e+15 ohm-cm
Surface Resistance 7.85e+15 ohm
Dielectric Constant 2.9
@Frequency 1e+6 Hz
 3.06
@Frequency 1000 Hz
 3.09
@Frequency 60 Hz
Dissipation Factor 0.0078
@Frequency 1000 Hz
 0.0089
@Frequency 60 Hz
 0.017
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °CDeflection temperature; load unknown.
 
Processing PropertiesOriginal ValueComments
Pot Life 240 min500 g
 
Descriptive Properties
Exotherm190°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Molded, Mineral Filled
Overview of materials for Epoxy, Cast, Unreinforced
Overview of materials for Epoxy Cure Resin
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulating Grade
Cosmic Plastics E4920D Mineral Filled Epoxy Molding Compound

PABDR1 / 21996

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.