Sandvik 25.22.2.LMn is a strip electrode commonly used in urea plants to obtain a 25Cr22Ni2Mo corrosion resistant overlay weld deposit on carbon, carbon manganese and low alloyed steels using submerged arc welding (SAW) with Sandvik 31S flux or electroslag welding (ESW) with Sandvik 47S flux. Since there are many possible combinations and conditions, consulting Sandvik for details and advice is recommended.Information provided by Sandvik |