MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant Natural Color Polycarbonate + ABS 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: Polycarbonate + Acrylonitrile Butadiene Styrene (PC+ABS) polymer blend is one of the most widely used engineering compounds that has high toughness, high impact strength and has high dimensional stability. Clariant optimizes PC+ABS with additives to achieve improved heat stability and resistance to thermo-oxidative degradation and yellowing.

General properties:

  • Strong and tough engineering thermoplastic
  • High impact strength
  • High heat resistance
  • Good low temperature ductility
Optimized benefits:
  • Reduced thermo-oxidative degradation
  • Minimized undesired yellowing due to ultraviolet light
  • Excellent flow characteristics
Applications:
  • Mechanical and technical application parts that require strength and toughness
  • Prototypes
  • Tools, jigs, fixtures

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.144 g/ccISO 1183
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
 20 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaInjection molded, 50 mm/min; ISO 527
Elongation at Break 34 %Injection molded, 50 mm/min; ISO 527
Flexural Strength 85.0 MPaInjection molded; ISO 178
Flexural Modulus 2300 MPaInjection molded; ISO 178
Izod Impact, Notched (ISO) 58.0 kJ/m²Injection molded; ISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 126 °CInjection molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 107 °CInjection molded; ISO 75
Glass Transition Temp, Tg 113 - 145 °CDSC; ISO 11357
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 285 °CPrint Temperature
Moisture Content 0.020 %after drying at 120°C for 2 hours; ISO 15512
 
Descriptive Properties
Bed Adhesiona thin coating of PVP glue on glass or carbon fiber
Bed Temperatureideally heated up to 110°C (use an enclosed chamber if possible)
Fan Settingslow
Print Speed20-50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Clariant Polycarbonate + ABS White 3D Printer Filament
Clariant Polycarbonate + ABS Red 3D Printer Filament
Clariant Acrylonitrile Butadiene Styrene Black 3D Printer Filament
Clariant Polycarbonate + ABS Black 3D Printer Filament
Clariant Natural Color Acrylonitrile Butadiene Styrene 3D Printer Filament

PCLAR00023 / 232100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.