System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Dow Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer
Categories:
Polymer
;
Thermoplastic
;
Ethylene Butyl Acrylate
Material Notes:
Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.
Availability:
Globally
Information provided by DuPont.
This former DuPont product line is now a Dow product line.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.940
g/cc
ASTM D792 - ISO 1183
Melt Flow
12
g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238 - ISO 1133
Mechanical Properties
Original Value
Comments
Hardness, Shore A
73
ASTM D2240 - ISO 868
Tensile Strength at Break
754
psi
ASTM D638 - ISO 527-2
Elongation at Break
950 %
ASTM D638 - ISO 527-2
Thermal Properties
Original Value
Comments
Melting Point
72.0
°C
ASTM D3418 - ISO 3146
Glass Transition Temp, Tg
-55.0
°C
ASTM D3418
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Dow Elvaloy® HP441 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
Dow Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer
Dow Elvaloy® AC 1330 Ethylene Methyl Acrylate
Dow Elvaloy® AC 2618 Ethylene Methyl Acrylate
PDUPM048 / 33715
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.