MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess LEWATIT® MonoPlus TP 220 Ion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® MonoPlus TP 220 is a macroporous weakly basic resin with chelating resin with bis-picolylamine groups for copper, nickel and cobalt processing solutions. It has a monodisperse bead size distribution, i.e. beads of a uniform size, which results in high adsorption kinetics and a good utilization of the theoretical capacity. The resin exhibits a very high osmotic and mechanical stability to meet the requirements of metal processing technologies. It is delivered in the protonated sulfate form and can therefore be used without pretreatment. Under acidic conditions (pH=2) heavy metal cations are removed from aqueous solutions consistent with the following selectivity series: Cu2>>Ni2>>UO2>Fe3>Co2>Cd2>Fe2. Lewatit MonoPlus TP 220 is especially suitable for the use in the following applications:
    Purification of cobalt electrolytes (cobalt/nickel separation)
  • Separation of nickel/copper from ferric solutions
  • Recovery of copper from strongly acidic solutions (pH <2)
  • Purification of chromium (III) baths (removal of heavy metals such as copper and nickel)
  • Adsorption of heavy metals (e.g copper) from solutions containing strong chelating agents like EDTA
While most metals are removed from the loaded resin with a conventional acid strip, copper can only efficiently be desorbed with ammonia solution.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.720 g/cc0.0260 lb/in³
Density 1.12 g/cc0.0405 lb/in³
Bead Size 0.570 - 0.670 mm0.0224 - 0.0264 inMean
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 70.0 °C158 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Appearanceopaque
pH Operating Range1 - 14

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8809 / 209201

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.